Batteries with Other Chemistries

Wednesday, 8 October 2014: 14:00-18:00
Sunrise, 2nd Floor, Galactic Ballroom 1 (Moon Palace Resort)
Chair:
Yangchuan Xing
14:00
99
Insights into the Solvation Structure of Multi-Valent Ions for Multivalent Battery Applications
K. A. Persson, N. N. Rajput, and X. Qu (Lawrence Berkeley National Laboratory)
14:20
100
High Energy Non-Aqueous Al-S Battery
G. Cohn and L. A. Archer (Cornell University)
14:40
101
Mxenes As High Capacity Electrodes Materials for Metal (Li, Na, K, Ca)-Ion Batteries
D. Er, J. Li (Dept of Mat. Sci. and Eng., University of Pennsylvania), M. Naguib, Y. Gogotsi (Dept of Mat. Sci. and Eng., Drexel University), and V. B. Shenoy (Depts of Mat. Sci. and Eng. & Mech. Eng. and App. Mech., University of Pennsylvania)
15:00
102
Redox Active Molecules for Non-Aquoes Flow Battery
L. Zhang (Argonne National Laboratory), J. Huang (Argonne National Lab, Argonne National Lab), and A. K. Burrell (Argonne National Laboratory)
15:20
103
Synthesis of Nickel-Cobalt Difluoride [NixCo(1-x)F2] for Lithium Ion Batteries Application
Y. T. Teng (TUM CREATE Centre for Electromobility, Energy Research Institute @ NTU (ERI@N)), F. Wei (Nanyang Technological University), and R. Yazami (Energy Research Institute @ NTU (ERI@N))
15:40
104
Aqueous Lithium-Iodine Battery
H. R. Byon (Byon Initiative Research Unit, RIKEN, Japan) and Y. Zhao (Byon Initiative Research Unit, RIKEN, Japan, Department of Mechanical Engineering and the Materials Science and Engineering Program, The University of Texas at Austin, USA)
16:00
105
Chloride Ion Batteries Based on Metal Oxychloride/Metal Electrode Systems
X. Zhao (College of Materials Science and Engineering, Nanjing University of Technology, China, Institute of Nanotechnology (INT), Karlsruhe Institute of Technology (KIT), Germany), P. Gao (Helmholtz Institute Ulm (HIU), Germany), Z. Zhao-Karger (Institute of Nanotechnology (INT), Karlsruhe Institute of Technology (KIT), Germany), M. Fichtner (Institute of Nanotechnology (INT), Karlsruhe Institute of Technology (KIT), Germany, Helmholtz Institute Ulm (HIU), Germany), and X. Shen (College of Materials Science and Engineering, Nanjing University of Technology, China)
16:20
106
Micro- and Mesoporous Carbon - Selenium Composite Cathode for Lithium / Selenium Battery
J. T. Lee, H. Kim (School of Materials Science and Engineering, Georgia Institute of Technology), M. Oschatz (Technische Universität Dresden), D. C. Lee, F. Wu, H. T. Lin (School of Materials Science and Engineering, Georgia Institute of Technology), W. I. Cho (Center for Energy Convergence, Korea Institute of Science and Technology (KIST)), S. Kaskel (Technische Universität Dresden), and G. Yushin (School of Materials Science and Engineering, Georgia Institute of Technology)
 
107
Electrochemical Insertion/Deinsertion of Mg2+ Ions into MnO2 Nanowires (Cancelled)
17:00
108
Beyond Chevrel Phase Mo6S8 : High Energy Density Mg Battery Cathodes
F. Mizuno, T. S. Arthur, R. Zhang, and C. Ling (Toyota Research Institute of North America)
17:20
109
Composite Block Copolymer Electrolytes for Lithium Metal Batteries
Y. G. Lee (Samsung Advanced Institute of Technology (SAIT), Samsung Electronics), Y. Yang, H. S. Choi, and J. N. Lee (Samsung Advanced Institute of Technology (SAIT),Samsung Electronics)