Sodium-Ion Anode

Wednesday, 16 May 2018: 08:00-12:00
Room 609 (Washington State Convention Center)
Chairs:
Xiulei Ji and Mallory Clites
08:40
445
09:00
446
Highly Defective Hard Carbon Anode for Na-Ion Batteries By Microwave Heating
Z. Li, Y. Chen, Z. Jian, H. Jiang (Oregon State University), J. Razink (University of Oregon), W. F. Stickle (Hewlett-Packard Co.), J. Neuefeind (Oak Ridge National Laboratory), and X. Ji (Oregon State University)
 
447
Expanded Biomass-Derived Hard Carbon with Ultra-Stable Performance for Sodium-Ion Batteries (Cancelled)
09:40
Break
10:00
448
Highly Stable Sodium Metal Batteries Enabled By High Efficiency Electrolytes
J. Zheng, S. Chen, W. Zhao, M. H. Engelhard, and J. Zhang (Pacific Northwest National Laboratory)
 
449
High Performance Na–CuCl2 Secondary Battery Using Sulfur Dioxide Based Inorganic Liquid Electrolyte (Cancelled)
 
450
Solid Electrolyte Interphase and Nitrogen Doping Effect on Potassium Storage Mechanism in Graphite (Cancelled)
 
451
Effect of Halide Doping on the Structure and Properties of Na3SbS4 Solid Electrolyte (Cancelled)
11:40
453
Enabling High Initial Coulombic Efficiency of Hard Carbon By a Pre-Lithiation Treatment for Sodium-Ion Batteries
B. Xiao, M. H. Engelhard, D. Reed, V. Sprenkle, and X. Li (Pacific Northwest National Laboratory)