Li-Ion Battery VI - System

Thursday, May 15, 2014: 14:00-17:40
Bonnet Creek Ballroom I, Lobby Level (Hilton Orlando Bonnet Creek)
Chairs:
Chuanbo Yang and Yangchuan Xing
14:00
154
Mathematical Model for a Spirally-Wound Lithium-Ion Cell
M. Guo (ESim LLC) and R. E. White (University of South Carolina)
14:20
155
Efficient Mass Conserving Reformulation Schemes for Nonlinear Solid-Phase Spherical Diffusion Equation for Lithium Intercalation
P. C. Urisanga (Department of Electrical and Systems Engineering, Washington University in St. Louis), P. W. C. Northrop, S. De (Department of Energy, Environmental and Chemical Engineering, Washington University in St. Louis), and V. R. Subramanian (Washington University-St. Louis)
14:40
156
Investigation of Consistency of Aging Mechanism inside a Batch of Commercial 18650 Cells
A. Devie, M. Dubarry, and B. Y. Liaw (University of Hawaii at Manoa)
15:00
157
In Situ Hard x-Ray Nano-Tomography Study of Lithium Ion Batteries
J. Wang, Y. C. K. Chen-Wiegart, and J. Wang (Brookhaven National Laboratory)
15:20
Break
 
158
Non-Uniformity Behaviors of Commercial Large-Format Batteries: Performance and Durability (Cancelled)
16:00
160
Cell- and Pack-Level Simulation of Large-Format Li-Ion Battery Safety Events
J. F. Kalupson, Q. Wang, W. Zhao, P. K. Sinha, C. E. Shaffer, and C. Y. Wang (EC Power)
 
159
Development of a Specialized 18650 Lithium Ion Cell and Automated Manufacturing Line in California, USA (Cancelled)
16:40
161
Post-Test Analysis of Battery Materials:  Another Part of the Question
I. Bloom, N. D. Rago, A. N. Jansen, B. J. Polzin (Argonne National Laboratory), S. E. Trask (Chemical Sciences and Engineering Division, Argonne National Laboratory), and J. Bareno (Argonne National Laboratory)
17:00
162
A Study on the Decomposition of Lithium-Ion Battery Electrolytes from Different Field-Tested Hybrid Vehicles
M. Grützke, V. Kraft, B. Hoffmann, S. Klamor, X. Mönnighoff (University of Münster, MEET Battery Research Center), M. Winter (MEET Battery Research Center, University of Muenster), and S. Nowak (University of Münster, MEET Battery Research Center)
 
163
From Lab Scale to Large Volume Production: Substitution of Toxic NMP/PVDF with H2o/CMC/SBR in Lithium-Ion Cells (Cancelled)