D2-1. Pt-Based Catalysts with Durable Suppports II

Wednesday, 8 October 2014: 08:00-12:20
Sunrise, 2nd Floor, Galactic Ballroom 7 (Moon Palace Resort)
Chairs:
Rod L Borup and Yu Morimoto
08:00
Evaluation of Durability with MEAs Made by Graphitized Carbon Supports
A. Hayashi (Kyushu University), X. Zhao (Faculty of Engineering, Kyushu University), Y. Minamida, M. Kitamura, Z. Noda, and K. Sasaki (Kyushu University)
08:20
Invited: Electrocatalyst Layer Degradation of PEM Fuel Cells
R. L. Borup, R. Mukundan, D. Spernjak, D. A. Langlois, D. Torraco (Los Alamos National Laboratory), K. L. More (Oak Ridge National Laboratory), R. Ahluwalia, S. Arisetty (Argonne National Laboratory), and L. Guétaz (CEA, LITEN, Département de l’Electricité et de l’Hydrogène pour les Transports, Laboratoire des Composants PEM, 17, Rue des Martyrs, 38054 Grenoble, France)
09:00
Improvements of Electrical and Electrochemical Activities at Nb-SnO2 Supports by Aggregation and Pt Loading as Fuel Cell Cathode Catalysts
K. Kakinuma (Fuel Cell Nanomaterials Center, University of Yamanashi), Y. Senoo (Corporate R and D Center, Mitsui Mining and Smelting@Co., Ltd., Interdisciplinary Graduate School of Medicine and Engineering, University of Yamanashi), Y. Chino (Interdisciplinary Graduate School of Medicine and Engineering, University of Yamanashi), K. Taniguchi (Corporate R and D Center, Mitsui Mining and Smelting@Co., Ltd.), M. Uchida (Fuel Cell Nanomaterials Center, University of Yamanashi), H. Uchida (Clean Energy Research Center, University of Yamanashi), S. Deki (Fuel Cell Nanomaterials Center, University of Yamanashi,), and M. Watanabe (Fuel Cell Nanomaterials Center, University of Yamanashi)
09:20
SnO2 As an Effective Protection Layer of Electrospun Carbon Nanowires Based Catalyst for PEMFC Applications
G. Ercolano (ICGM, Aggregates, Interfaces and Materials for Energy, CNRS Montpellier, France), C. Marichy (Laboratoire des Multimatériaux et Interfaces, CNRS-Université Lyon 1), R. M. Silva (CICECO, University of Aveiro), G. Caputo (Institut für Chemie, Humboldt Universität zu Berlin), D. J. Jones, J. Roziere, S. Cavaliere (ICGM, Aggregates, Interfaces and Materials for Energy, CNRS Montpellier, France), and N. Pinna (Institut für Chemie, Humboldt Universität zu Berlin)
09:40
Intermission
10:00
Understanding the Growth of Pt Nanoparticles by Galvanic Displacement on ITO Nanocubes for ORR
Y. Liu, S. Zhao, and W. E. Mustain (University of Connecticut)
10:20
Alternative Oxide-Supported PEFC Electrocatalysts
K. Sasaki, Z. Noda, T. Tsukatsune, K. Kanda, Y. Takabatake, Y. Nagamatsu, T. Daio, S. M. Lyth, and A. Hayashi (Kyushu University)
10:40
Doing More with Less: Challenges for PEMFC Catalyst Layer Design
J. Stumper (Automotive Fuel Cell Cooperation Corporation)
11:00
Fabrication and Cell Analysis of a Pt/SiO2 Platinum Thin Film Electrode
M. Inaba, T. Suzuki, T. Hatanaka, and Y. Morimoto (Toyota Central R&D Labs., Inc.)
11:20
The Stability of Nano-Structured-Thin-Film™ Supported Ir on Pt PEMFC Catalysts Under Rde Simulated Start-up and Shut-Down
T. C. Crowtz (Dept. of Process Engineering and Applied Science, Dalhousie University), R. Sanderson (Dept. of Physics and Atmospheric Science, Dalhousie University), and J. Dahn (Dalhousie University - Dept. of Physics and Atmospheric Science)
11:40
The Impact of Pretreatments and Conditioning on the Structure and Performance of NSTF ORR Alloy Catalysts
D. A. Cullen, K. L. More (Oak Ridge National Laboratory), J. Erlebacher (Johns Hopkins University), D. van der Vliet, S. M. Luopa, and A. J. Steinbach (3M Company)
12:00
Pt Catalysts Supported on Polybenzimidazole-Grafted Graphene for PEMFCs